Effect of Warm Compaction and Lubricant on Microstructure and ...
Then, in a planetary ball mill, Mo prealloy powder, Cu, C, and the selfmade composite lubricant were mixed with a ball material ratio of 1:1 and rotated at a speed of 300 rpm for 60 min to obtain the mixed powder. The amount of lubricant added was,,, and wt.%.